It looks as if the frame is ruined. It almost never is. Reading time: 3'
What the white film is

Cellulose acetate is cellulose plus a plasticiser, the ingredient that keeps the material flexible instead of brittle. Over time, and much faster with heat or solvents, some of that plasticiser migrates to the surface and sets there as a fine, dull, whitish layer. Frame makers call it bloom. It sits on the outside of the material, a few hundredths of a millimetre deep, and the acetate underneath is unchanged. That is why it can be removed.
Before you assume bloom, rule out the other thing that looks exactly like it: a film of sunscreen, sweat and skin oil that has dried onto the frame. Wash it first.
What causes it
Heat is the big one. A frame left on a dashboard, a radiator or under a hairdryer blooms within days. Chemicals are second: alcohol, hand sanitiser, hairspray, perfume, sunscreen and insect repellent all carry solvents that pull plasticiser out of the surface where they sit. Age is third; a frame from the seventies may bloom simply because it is fifty years old. And acetate that was cut before it had finished curing blooms sooner than acetate that was left to rest. What cured acetate means.
Step one: wash it
Lukewarm water, a drop of dish soap, fingertips, rinse, dry with the microfibre cloth. If the haze disappears, it was residue, and the fix is to wash the frame more often in summer. If it is still there when the frame is dry, it is bloom.
Step two: the polishing wheel
Any optician has one. The frame goes against a soft wheel with polishing compound for a few minutes and the bloomed layer comes off, taking the gloss back to the day it was made. It is a ten-minute job and most opticians charge little or nothing for it. Hinges and lenses are untouched.
Do not try to do this at home. Toothpaste, baking soda and car polish are abrasives that leave a web of fine scratches you then cannot remove. Acetone and nail-polish remover dissolve acetate outright. Oils and balms hide the haze for an hour by filling it, then attract dirt.
Will it come back
Only if the cause does. Keep the frame out of hot cars, spray hair and sunscreen before you put the glasses on, wash the frame with water and soap, and a polished frame stays clear for years. Frames cut from cured sheet are the slowest to bloom in the first place.
When it is more than bloom
Two signs mean the material itself is going. A network of fine cracks in the surface, usually around the hinges and the bridge, is crazing: the acetate has lost plasticiser all the way through and has gone brittle. And a smell of vinegar from the frame is acetic acid being released as the material breaks down. Both are rare in frames under twenty years old and common in neglected vintage ones. A crazed frame can still be polished, but it will not survive another adjustment, so handle it gently. What to check before buying vintage.
SWT frames are cut from cured acetate and polished by hand, which is the best start a frame can have. If a pair of ours ever dulls, any optician brings it back. How to clean and store acetate, and what acetate looks like when it ages well.
Questions people ask
Is the white film harmful?
No. It is the frame's own plasticiser, on the surface. It is a cosmetic problem, not a safety one.
Does bloom mean the frame was cheap?
Not on its own. Any acetate can bloom if it is left in a hot car. Uncured acetate blooms sooner and more often, which is one reason cheaper frames go cloudy first.
Can I use olive oil or petroleum jelly?
They fill the haze and make it disappear for an evening, then attract dust and come back worse. Polishing is the fix.
How often should a frame be polished?
When you notice it has dulled. For a frame kept in its case, that is every few years, if at all.
|
SWT Eyewear Cured acetate, polished by hand. Made to be kept. |